UV Curing Polyurethane Acrylic Coatings for Glass
Author(s): 
Pages: 15-17
Year: Issue:  2
Journal: PAINT & COATINGS INDUSTRY

Keyword:  紫外光固化聚氨酯丙烯酸酯玻璃涂料硅烷偶联剂红外光谱;
Abstract: 研制了紫外光固化的玻璃涂料.研究表明,在漆膜厚度为100μm的情况下,2 kW的高压汞灯辐射固定距离为7 cm,预聚物与单体的比例为7:3,添加0.5%的硅烷偶联剂,固化时间为30 s,其综合性能最好.用FITR表征了固化前后的结构.