ti gao 16mn lian zhu pi zha zhi hou ban de he ge lv
Author(s): 
Pages: 26-29
Year: Issue:  3
Journal: Continuous Casting

Keyword:  连铸坯合格率厚板中板轧制裂纹敏感性裂纹废品铸坯表面温度电炉冶炼表面缺陷氧化铁皮;
Abstract: 本文分析了造成电炉冶炼的16Mn连铸坯轧制厚板合格率低,出现裂纹与凹坑等废品的原因,并提出了相应措施。这些措施采用后,取得了满意效果和显著的经济效益。