Corrosion characteristics and protection of transmission iron tower
Author(s): 
Pages: 24-26,42
Year: Issue:  3
Journal: Hunan Electric Power

Abstract: 分析株洲铜清地区输电铁塔的腐蚀特征,指出SO2酸性气体是造成腐蚀的主要因素,腐蚀的起源点为镀锌层损坏处和塔材边角部位,而防腐涂料选用不当、涂刷工艺不良加速腐蚀.提出输电铁塔腐蚀防护的通用要求、腐蚀评判准则、改造技术要求和涂料选择要求,规范腐蚀防护工作.