Effects of several minor elements on superalloys and their mechanism
Author(s): GUO Jian-ting
Pages: 465-
475
Year: 2011
Issue:
3
Journal: The Chinese Journal of Nonferrous Metals
Abstract: 研究几种微量元素对高温合金力学性能和微观组织结构的影响;从晶界结合力、晶界沉淀和凝固偏析等方面对微量元素的不同作用进行讨论.结果表明:适量的B、C、Y、La、Ce、Zr和Mg明显改善高温合金的持久性能;Si和S则明显降低高温合金的持久性能;而P对一些高温合金特别是变形高温合金表现出有益作用,而对另一些高温合金特别是铸造合金表现出有害作用.