Microstructure Evolution of Magnesium Alloy AZ91D Refined by Sr Addition During Partial Remelting
Author(s): 
Pages: 9-12
Year: Issue:  23
Journal: Hot Working Technology

Keyword:  AZ91D镁合金Sr半固态合金部分重熔;
Abstract: 研究了添加微量Sr细化的AZ91D镁合金部分重熔过程中的组织演变.考察了加热温度和等温时间对合金初生相形态和尺寸的影响.结果表明:添加质量分数为0.1%的Sr,在610℃浇注的AZ91D镁合金部分重熔后,可以获得初生相为球状或粒状的非枝晶半同态合金,基本具备触变过程所需要的组织状态;等温时间一定时,随着重熔温度提高,半固态组织球化过程加快,但加热温度过高,试样表面有大量液相渗出,并在自重作用下严重变形;当重熔温度一定时,随等温时间延长,初生相变得愈加膪l整,但等温时间过长,初生相有长大倾向.