Preparation of Double-Cationic Modified Coatings by Microfluidiser Comminution Method and Its Application
Author(s): 
Pages: 28-31
Year: Issue:  4
Journal: Paint & Coatings Industry

Keyword:  改性涂料粒径Zeta电位稳定性染色深度牢度;
Abstract: 采用微射流法用Gemini双阳离子分散剂制备双阳离子化改性涂料.在Gemini双阳离子分散剂用量为1%,涂料用量为5%,微射流分散时间为30 min,微射流分散压力为1.7×105kPa条件下制备的双阳离子化改性涂料的粒径为211.9 nln,Zeta电位为32.4 mV,黏度为1.33 mPa·s.结果表明,双阳离子化改性涂料具有较好的贮存稳定性和酸碱稳定性,用于染色后织物的K/S值较常规未改性涂料提高了16.2%,各项牢度可以提高半级以上.